airair
Sr Member
Thanks airair. Weren't you doing one of these as well? Something about an 80 shore material?
ive got the castings i did, the original piece was in clay and it crumbled.
So what I could do is grind one of the castings and reshape it slightly.
its quite close, but needs shaving on a few areas and then maybe making it a bit hollow.
I used that rubber casting material, think pt flex 85, which is too hard really, it can be made much softer.
I might give it a go again soon.