Re: Foam Jaffa Horus guard headdress.
Thank you all for the great compliments They are really appreciated.
As for living in the LA area, afraid not, I am in a small town called Atikokan in Ontario. The thickness of the foam I used for this build is 5mm roll. For some of the raised details I just used craft foam I believe it is 2 mm thick. Which reminds me I still have some raised detailing to do, I better get that done.
I went for close accuracy, lol. Some of the detailing is different but overall I think it is recognizable.
Unfortunately painting will have to wait a week or two, it is way to cold here still to doing any painting, I do not have a shed or workshop so it all has to be done outside and it is -13 (-20 with the wind chill).
I am hoping to do a gold/bronze type finish on it.