WOW THIS IS AN OLD THREAD!!!
Just to add my 2 cents to this. I put some upol fantastic on my iron man build on Saturday.... OK thats a slight lie, I also mixed it with resin to thin it a bit, it went like yoghurt, great to apply. So smooth, AMAZING!!!
aNYWAY... AdDed the filler catalyst and the resin catalyst just to make sure it went off. Gave it a real good mix for ages. The weather is very cold herE in the UK at the moment so I knew it would take a while to cure. I have come back to my shed today (3 days later) to find a kind of rubbery gloopy coat on my beloved MK7 chest.
Terrified, I've been doing some epic searching all over google and I came across this thread and another saying just slam some heat into it. Ive had it in front of my heater for half an hour, until it was way to hot to touch and I can confirm that it has now cooled down and cured just nicely.
I can also confirm that I didn't ventilate, and I literally feel high as a kite. Not good for recreational purposes... don't try it!
Anyway, all in all, positive experience. Just heat it up until you cant tough it, then let it cool down. Only do this if you cant be arsed to restart your piece... like me.
ALSO!!!! Ventilate! Anyway I'm off to throw up. ~
In case this stuff is highly toxic... May my legacy live on in this post.
Peace out!!!!